Re: [MW:29084] Hardness for SA516 Grade 70

This 200HB is only mentioned as in delivery condition, not in as welded condition.

As welded hardness depends on chemistry and cooling rate (e.g preheat, heat-input, wall thickness)
Regards

Jurgen Prinsen IWE/MSc
Weld-Tech BV

Welding consultancy and engineering since 1988


Van: "JosƩ Juan JimƩnez Alejandro" <jjjimeneza@gmail.com>
Aan: materials-welding@googlegroups.com
Verzonden: Zondag 10 februari 2019 18:09:34
Onderwerp: Re: [MW:29081] Hardness for SA516 Grade 70

I was looking for that data in the Code, I could not find it, hopefully someone has better luck and share the hardness data of this steel, with reference to the standard; On the other hand, when a pressure vessel carries the ASME stamp, the Authorized Inspector of the Authorized Inspection Agency necessarily has to intervene with your company has a contract, the Authorized Inspector has the obligation to advise and give you technical support.

El dom., 10 feb. 2019 a las 6:42, BCK 055 (<bck055@gmail.com>) escribió:
PWHT is followed spec, and WPS should be shown hardness test value.

Sent from my Blackberry
From: RKD
Sent: Sunday, February 10, 2019 17:52
To: Materials & Welding
Subject: [MW:29073] Hardness for SA516 Grade 70


For a pressure vessel designed with stamped under ASME VIII Div.1, there is a requirement that: "Hardness values should not exceed 200 brinell for the welds / material of shell."


Shell material is specified as SA516 Grade 70.


I am concerned the requirements for hardness and material will automatically require stress relief for all pressure vessel parts.


Would SA516 Grade 70 have hardness lower than 200 Brinell?


Thank you.


Regards,

RKD


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

Ing. JosƩ Juan JimƩnez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...