Re: [MW:29076] Hardness for SA516 Grade 70

PWHT is followed spec, and WPS should be shown hardness test value.

Sent from my Blackberry
From: RKD
Sent: Sunday, February 10, 2019 17:52
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:29073] Hardness for SA516 Grade 70

For a pressure vessel designed with stamped under ASME VIII Div.1, there is a requirement that: "Hardness values should not exceed 200 brinell for the welds / material of shell."


Shell material is specified as SA516 Grade 70.


I am concerned the requirements for hardness and material will automatically require stress relief for all pressure vessel parts.


Would SA516 Grade 70 have hardness lower than 200 Brinell?


Thank you.


Regards,

RKD

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...