Re: [MW:29075] grain size requirements for 321H stainless steel

Lower grain size (e.g. 6, 5, 4 and so on) are coarser

Thanks & Regards,
Jay Poojary

On Sun, Feb 10, 2019, 4:22 PM sandeep kumar <sandeepdhiman63@gmail.com wrote:
Dear all

Please advise your views on below query:

ASTM A182 10.1.2 Grades F 321H, F 347H, and F 348H shall have a
grain size of ASTM No. 7 or coarser.


What does it stand for coarser? 
Does it mean a higher ASTM grain size no (e.g. 8, 9 and so on) or lower ASTM grain size no. (e.g. 6, 5, 4 and so on)?


Thanks & regards
Sandeep 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...