Re: [MW:28890] EN 10204 Type certificate

Dear.

If manufacturer doesnt shown certificate type 3.1 then by doing check test to confirm 3.1 is acceptable.

Regards

Dinesh

On 3 Jan 2019 18:41, "vk" <vivekmohan007@gmail.com> wrote:
Gents,

Manufacturer has issued MTC fulfilling all the requirements as mentioned in EN 10204 3.1.

But nowhere it mentions as "EN 10204 Type 3.1"

Can this be considered or do they have to mention that it complies with the requirements of EN 10204 Type3.1"

Regards
Vivek

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...