Please advice.. sir
On 27 Dec 2018 14:05, "Dinesh Somwanshi" <som.din@gmail.com> wrote:
-- Dear sir,I needed advice, along with Reference code for EIL specs Jobs.a) I received plate from X mill, While verifying MTC it has been observed that 1 tensile test has been provided, While code requirements of 2 tensile test.How we can proceed for MTC approval with check test? ( either 1 additional test of Tensile or 2 tensile )B) I received plate from X mill, While verifying MTC it has been observed that for 310S, content of MO missing in MTC as per code has requirement of MO .How we can validate to proceed for MTC approval with check test ?( either 1 chemical content of MO / full content chemical analysis / Both tensile Chemical)Please Advice.Thanks & RegardsDINESH VITTHAL SOMWANSHI
BACHELOR IN MECHANICAL ENGINEER
असो द्यावी दया तुमच्या लागतसे पाया.
*Pray for others, sometime, You might never need to pray for yourself
again.....*
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment