Dear Noor,

It all depends on the code,
If it is acc. to ASME IX with no impacts requirements there is no problem, because they are all P1
If supplementary essentials are involved the Gr. nr is an issue.

If is is acc. another code, or spec, please look in detail for the requirements

Regards


Jurgen Prinsen MSc/IWE
Weld-Tech BV
Welding Engineering and Consultancy


Van: "Noor Osama" <noorkathir@gmail.com>
Aan: "Materials & Welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 25 oktober 2018 09:35:24
Onderwerp: [MW:28498] Using API 5LX65 FLG instead of A350 LF2 during qualification of A333 GR 6 P1G1 to P1G2

Dear Expert,

Is it possible to replace LTCS Flange A350 LF2 by Flange API 5L X65 during qualification of A333 GR 6 Pipes to A350 LF2 Flange.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...