Thursday, January 10, 2019

Re: Re: [MW:28885] Welding of Materials A333 Gr.6 to A516

Hi dear,
There is no need for a new WPS. A333 is P No.1 & A516 is also P No.1. A516 Gr 70 is better @ a lower temp. BUT TAKE CARE A516 is a plate, not a pipe and A333 is a pipe.

On Thu, Jan 10, 2019 at 2:24 PM muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (muneebslsa@gmail.com) Add cleanup rule | More info
Greetings,

Subject grade matters here, yes if 70 which is equivalent.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2019-01-10 00:01
Subject: Re: [MW:28882] Welding of Materials A333 Gr.6 to A516
no need to go for new procedure

On Wed, Jan 9, 2019 at 9:39 PM Andy <andrewgeraldmunro@gmail.com> wrote:
Good Afternoon, 

I'm looking for a bit of Guidance on Steel grades -

I have a welding procedure that covers me for ASTM A333 Gr.6 / ASTM A350 LF2 or Equivalent Grades. 

Can anybody advise if A516 is included in this equivalent grade or would i require a new procedure?

I feel that this "equivalent grade" Is open to interpretation. 

Thanks 
Andy

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Thanks & Regards
Hisham Al. Mohammad
Welding Engineer & QA/QC Engineer
Mob: +971 56 433 7326 & +971 52 667 9935

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...