Thursday, January 10, 2019

Re: [MW:28885] Welding of Materials A333 Gr.6 to A516

Dear Andy 

It all depends on the code,
If it is acc. to ASME IX with no impacts requirements there is no problem, because they are all P1
If supplementary essentials are involved the Gr. nr is an issue.

If is is acc. another code, or spec, please look in detail for the requirements

Regards


Jurgen Prinsen MSc/IWE
Weld-Tech BV
Welding Engineering and Consultancy


Van: muneebslsa@gmail.com
Aan: "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 10 januari 2019 05:18:09
Onderwerp: Re: Re: [MW:28884] Welding of Materials A333 Gr.6 to A516

Greetings,

Subject grade matters here, yes if 70 which is equivalent.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2019-01-10 00:01
Subject: Re: [MW:28882] Welding of Materials A333 Gr.6 to A516
no need to go for new procedure

On Wed, Jan 9, 2019 at 9:39 PM Andy <andrewgeraldmunro@gmail.com> wrote:
Good Afternoon, 

I'm looking for a bit of Guidance on Steel grades -

I have a welding procedure that covers me for ASTM A333 Gr.6 / ASTM A350 LF2 or Equivalent Grades. 

Can anybody advise if A516 is included in this equivalent grade or would i require a new procedure?

I feel that this "equivalent grade" Is open to interpretation. 

Thanks 
Andy

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...