Re: [MW:28845] Re: Calculation for root gap according to tihckness of pipe

Root gap is not dependent on pipe size or thickness. For the GTAW process the root gap is generally listed as 1/8 of an inch plus or minus 1/32 inch. in the WPS. For stainless steel open butt welding with the GTAW process this root gap will be increased due to shrinkage issues. Remember, one could run a PQR using 1/32 in. open root or 1/16 in. open root or a 5/32 inch open root and it will pass. The general standard in the U.S is 1/8 in. plus or minus 1/32 inch. Most good GTAW welders can handle this root gap. 



Gene Matsko


On ‎Tuesday‎, ‎January‎ ‎1‎, ‎2019‎ ‎04‎:‎14‎:‎27‎ ‎AM‎ ‎CST, Mohd Siraj <mohd52100@gmail.com> wrote:


Root gap is  not depend on pipe size or thickness,indeed it is based on process to be used for welding.
GTAW-4-5mm
SAMW-3.5-4.5mm
SAW-1.5-2.5mm

On Friday, July 22, 2011 at 2:17:46 PM UTC+3, abhishek ojha wrote:

Dear Expert,

Kindly guide me how to calculate root gap according tihckness of pipe of different /same dia.(different tickness but same dia)


Thanks & Regards,

 

Abhishek Ojha


 Engineer- Construction 


cid:image001.gif@01CA0B94.B49995B0

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...