Re: [MW:28845] Re: Calculation for root gap according to tihckness of pipe

Hi,

Refer 328.4.3 of ASME B 31.3 and fig 328.4.2 and same as B 31.3 also refer B16.25.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
From: Mohd Siraj
Date: 2019-01-01 13:38
Subject: [MW:28836] Re: Calculation for root gap according to tihckness of pipe
Root gap is  not depend on pipe size or thickness,indeed it is based on process to be used for welding.
GTAW-4-5mm
SAMW-3.5-4.5mm
SAW-1.5-2.5mm

On Friday, July 22, 2011 at 2:17:46 PM UTC+3, abhishek ojha wrote:

Dear Expert,

Kindly guide me how to calculate root gap according tihckness of pipe of different /same dia.(different tickness but same dia)


Thanks & Regards,

 

Abhishek Ojha


 Engineer- Construction 


cid:image001.gif@01CA0B94.B49995B0

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...