Gents,
-- Manufacturer has issued MTC fulfilling all the requirements as mentioned in EN 10204 3.1.
But nowhere it mentions as "EN 10204 Type 3.1"
Can this be considered or do they have to mention that it complies with the requirements of EN 10204 Type3.1"
Regards
Vivek