Thursday, January 3, 2019

Re: [MW:28861] Re: Material certification EN 3.1 OR 3.2 ?

Hi Siraj,
Please be informed that here requirement is for 3.2 certification. Whenever there is requirement of certification by third party it is 3.2. 
Hope, it is clear.

Thanks,
Warm Regards,

Rajnish Dixit


On Tue, Jan 1, 2019 at 13:00, Mohd Siraj
<mohd52100@gmail.com> wrote:
EN 3.1

On Monday, December 24, 2018 at 1:39:23 PM UTC+3, shaikh ahmed wrote:
Dear Expert,

Please can you advise on below snap shot of Specification asking for EN 3.2 Material certification correct me ?

it calling for EN 3.2 OR 3.1

image.png

thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...