Replica will give macrostrure, not micro

Best Regards,

Shashank C Vagal



On Sunday, 30 September, 2018, 12:30:08 PM IST, pradip kumar Sil <pradipsil@gmail.com> wrote:


Go for replica test

On Sun, 30 Sep 2018, 11:44 Ali Asghari, <asgharialigl@gmail.com> wrote:
Dear All.

Does anybody know how it is possible to evaluate the bainite or martensite of the base metal is tempered or not?
I want to know the method , frequency of testing, acceptance( such as figures) and any other issues that can say with confidently we have tempered micro structure or not?
as you know this is more crucial in sour service and is a requirement in our specification but doesn't mention detail of it.

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...