Re: [MW:28356] Water Vapour in welded joints

Pl. check. There can not be water vapour after welding. You can see side wetting (on either end of bead toes) and it is normal in SS welding due to certain chemical used in flux coating. It gets dried on its own.

C Sridhar.
---------------------

On Friday, 28 September, 2018, 11:18:32 AM IST, Hareesh K V <hareesh13h@gmail.com> wrote:


Boxbe This message is eligible for Automatic Cleanup! (hareesh13h@gmail.com) Add cleanup rule | More info
Dear Veterans, 

After the cooling of weld joints, water vapor is seen in the surface of weld joints. What is the reason? This is particularly seen in SS welded joints. 

Regards, 

Hareesh K V
+91-8547859202

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

I'm protected online with Avast Free Antivirus. Get it here — it's free forever.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...