Re: [MW:28343] PQR usage (SA 516 Gr. 70 to SA 36)

Yes

On Wed, 26 Sep 2018 3:30 pm williams p wilson, <williamswilsonp@gmail.com> wrote:
Dear All,

I Have a PQR for SA 516 Gr.70 (N) Plate with Charpy V-notch Test -20 degree C
Can we use this as a supportive PQR for SA 36 Welding Procedure Specification.
(No Impact Test)
Welding Position, Process , Consumables will be same.
No PWHT.

Thank You & Regards
Williams
Mechanical Engineer
P Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...