Hi friend
Latest eddition of 2017 Now.407.4 is deleted means earlier clause is not applicable or valid
Regards
Hegde


On Fri, 21 Sep 2018 at 17:24, George Dilintas
<dilintas@gmail.com> wrote:
it is still valid 
check this web site: cstools.asme.org

Στις Σάβ, 4 Αυγ 2018 στις 10:16 π.μ., ο/η Aslam Khan <aslamkhan15@gmail.com> έγραψε:
Dear Experts,

Is interpretation: IX-01-17 is still valid, if not, then how it affects this interpretation.

Intepretation: IX-01-17

Background: A groove weld procedure qualification test coupon 1.5 in. thick was welded with SMAW process using multiple passes of 1/2 in. thickness. The coupon was given a subsequent PWHT exceeding the upper transformation temperature prior to the completion of mechanical testing .

Question: May this PQR be used to support  the weld of partial penetration groove welds per QW-202.2(b) or weld repair and build-up welds per QW-202.3(b) on base material thickness exceeding 1.65 in.

Reply: No. Per QW-407.4, a procedure qualification test coupon receiving a PWHT in which the upper transformation is exceeded, the minimum qualified thickness for production welds is 1.1 times the thickness of the test coupon.

Regards,
Aslam Khan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...