Friday, September 21, 2018

Re: [MW:28309] need some help related QW 381 clause

assume that a welder has to deposit an overlay on a curved surface. If he is depositing that on the longitudinal direction, then the limitation on diameter is not applicable. If he is depositing the overlay in the circumferential one, then the limitation is applicable

Στις Τρί, 18 Σεπ 2018 στις 9:22 π.μ., ο/η ali <adeelscet@gmail.com> έγραψε:
Dear Experts,


I am beginner and  reading  asme ix for first time 
Please explain the highlighted portion of qw 381  in pic below... please explain a little bit in detail
Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.