in some cases the application Code requires impact test only on weld metal and not in HAZ. The supplementary essential variables are relevant to impact test on weldments  and not specific to HAZ impact test

Στις Κυρ, 5 Αυγ 2018 στις 1:35 μ.μ., ο/η Aslam Khan <aslamkhan15@gmail.com> έγραψε:
Dear Experts, 

Please explain this interpretation, it will be very helpful for me..

Interpretation:IX-13-01

Question: Does QW-403.6 apply when the HAZ isn't subject to impact testing such as when qualifying a P8 material.
 Reply: Yes

Why QW-403.6 still applies when there is no impact testing...

Regards..

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...