Wednesday, September 19, 2018

Re: [MW:28303] need some help related QW 381 clause

Last statement you have to read in conjunction starting from "When Specified as essential....".
Meaning diameter restriction will apply only if specified and restriction will only be applicable for overlay done in circumferential direction.

On Tue, Sep 18, 2018 at 10:22 AM ali <adeelscet@gmail.com> wrote:
Dear Experts,


I am beginner and  reading  asme ix for first time 
Please explain the highlighted portion of qw 381  in pic below... please explain a little bit in detail
Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...