Re: [MW:28280] RE: 28278] Query for WPS P1 to P8 weld joint

Yes you can

Sent from my iPad

On 15-Sep-2018, at 06:33, PGoswami <pgoswami@quickclic.net> wrote:

If the design and qualification codes are only ASME , then on the basis of Sec –IX, QW-250 & other clauses , yes.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of JAYAPAL DHAKSHNAMOORTHY
Sent: September 14, 2018 1:54 PM
To: materials-welding@googlegroups.com
Subject: [MW:28278] Query for WPS P1 to P8 weld joint

 

Dear experts,

 

I have qualified PQR of {SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 304L(P8 Gr1)} electrode used E309L(F no.-5&A no.8)(without PWHT ) condition.

 

Now i have job {(SA 516 Gr 60(P1 Gr 1) to (SA 240 TP 316L(P8 Gr 1)} 

& I have a electrode E309LMo(F no.-5&A no.8)(without PWHT ) condition. The above PQR suitable for to make the WPS for this process?.

 

 Regards.

 

DHAKSHNAMOORTHY.J

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...