Adeel,

 

SA517 Gr B is Q&T steel, with very high tensile strength . Selection of welding consumables matters a lot on the design conditions. Go to the web page of this group. Type in SA 517 in the search box, you'll find tons of discussions and answers.

Welding of this steel is not easy. Hence don't adopt hit and miss approach. Get a knowledgeable  welding engineer to help your organization.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of adeel
Sent: September 13, 2018 8:46 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:28274] how to select filler metal for a specific Material according to ASME Sectionv IX

 

Please sir expalin about asme section ... how to select electrode


On Thursday, September 13, 2018 at 4:15:17 PM UTC+5, Tajuddin mohammed wrote:

Please kindly refer API 577 there is one table for selection of filler material 

 

On Wed, 12 Sep 2018, 16:47 adeel, <adee...@gmail.com> wrote:

Dear Experts,

 

Please answer this question 

 

For example designer selected a material SA517 Gr B for work.

 

I went to to table Q/QB 422 for P no. & G no. ... I found P no. is 11B and G no. 4. 

 

Then i went to Section ii Part A where i found SA 517 Material is alloy steel and its SFA no. is 5.5.

 

After that what shuould I do ?

 

 experts (Who has thorough of ASME Section IX) please tell me step  by step how to select exact filler material. from section ii part C.

 

I shall be very thankful to All of you for this act of kindness.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...