Dear Sir,
 It depends upon the thickness of weld. 


My request to all the friends , when you are asking question, please mentioned the following details very clearly,
1. Reference/ Design code.
2. Material details
3. Services (line)
4. Sketch if any
5. Weld details


On Sunday, 16 September 2018 12:22:29 UTC+5:30, nishanth km wrote:
Dear sir,

For primary support which is directly welding to the pipe required pwht or not?

Please advice


Regards,

Nishanth km

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...