Thanks. the image is interesting.
-- However, there is no crack in the welding. and its looks away from typical HAZ area. The reason might be high restraint.
Thanks & regards
Sandeep Kumar
On Tuesday, August 14, 2018 at 3:17:11 PM UTC+3, nguyen tuan wrote:
On Tuesday, August 14, 2018 at 3:17:11 PM UTC+3, nguyen tuan wrote:
Dear Expert,The Cracking found on welded P91 to 50 Cr 50 Ni with welding consumable E NiCrFe-3If anyone has the comment on thisThanks ,Best Regards,Nguyen ANh Tuan