Thursday, June 7, 2018

Re: [MW:27942] ISO 15614 -1 (base metal and weld metal Qualification thickness)

Process 1 &2

 Range of base metal and weld metal are same.

in 2 case
Deposited weld for GTAW-5mm, SMAW-10mm
 Range Of base metal and weld metal
GTAW--- 2.5mm to 10mm
SMAW---5mm to 20mm.

since your base metal is 15mm which is greater than 12 mm, u should not use case 1. pl see again Table 5.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Jun 6, 2018 at 10:50 AM, sela <mechselastine@gmail.com> wrote:
Dear experts

As per ISO 15614  ... Table 5

PQR plate thickness is 15 mm

Case 1:

For GTAW, deposited thickness is 5 mm .     So qualified range is from to 10 mm (multi-run).
For GMAW, deposited thickness is 10 mm .   So qualified range is from 3 to 20 mm (multi-run).

For thickness of base metal, acc. to ISO 15614-1, table 5 is 3 to 30mm. weldmetal qualified thickness also 3 to 30 mm

Case 2:

For GTAW, deposited thickness is 5 mm .     
For GMAW, deposited thickness is 10 mm.   

For thickness of base metal, acc. to ISO 15614-1, table 5 is 7.5 to 30mm

Please answer which case is correct case1 or case 2??

Please give explanation?

Regards 

Selas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...