Re: [MW:26816] VALIDATION OF THE WELDING PROCESS FOR THE HARD FACING AND SEAT RING OF THE GATE VALVES

Dear Friend,

For validation of welding WPS and PQR is sufficient.
if the client is asking the process of validation you have to submit the trial records of WPS like proposed WPS and its records. The trial record should contain the parameters of welding and consumables process considering welder and equipment are qualified. this records may be supplied until the aimed result is obtained.

For Ex:
Trial No        parameters        consumables               result                            remark
1                    xxxxxxxx            xxxxxxxxxx          Not satisfactory                    xxxxx
2                    xxxxxxxx               xxxxxxxx            Satisfactory                           xxxx


Regards,

Anosh Wankhade



From: "Nachhattar Singh" <nachhattar1947@gmail.com>
Sent: Thu, 31 Aug 2017 11:36:49
To: <materials-welding@googlegroups.com>
Subject: [MW:26775] VALIDATION OF THE WELDING PROCESS FOR THE HARD FACING AND SEAT RING OF THE GATE VALVES

Dear Experts

 

I am required to submit to the client as to how the “VALIDATION OF THE WELDING PROCESS FOR

THE HARD FACING AND SEAT RING WELDING OF THE GATE VALVES” will be done. Following has already

Been complied and submitted but the client wants some more to be done:-

 

01.   WPS is accepted as submitted.

02.   PQR based on the WPS is in place and accepted.

03.   Heat treatment is not the requirement.

 

Please advise what else should be done, give the reference of such requirements.

 

Thanks in advance

 

NS Gurm

 

PLEASE THINK BEFORE PRINTING

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .