Friday, February 12, 2016

Re: [MW:24272] Alloy Material P22, A335 (Cr2.25 and Mo 1)

In your case the governing thickness is that of the fillet ‎weld of the shoe to the pipe weld.
Min. Thickness for which PWHT is required depends on design and construction Code

Sent from my BlackBerry 10 smartphone.
From: 'nawab ali bhatti' via Materials & Welding
Sent: Παρασκευή, 12 Φεβρουαρίου 2016 - 07:12
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:24268] Alloy Material P22, A335 (Cr2.25 and Mo 1)

Dear Experts

Please   share your best  experience  with reference of international codes

Pipe Material  P22, A335 (Cr2.25 and Mo 1), Shoe support to be welded direct with pressure parts.(Pipe material thickness 33 mm, Operating Temperature 500 Centigrade  and pressure 106 bar)
 
My question,   Is  PWHT require for shoe supports  Or Not???
                     Shoe support plate thickness is 12 mm and throat thickness is 8 mm, Preheating is perform as WPS.


NA Bhatti
00966 593530001



                     

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/241801168.2167526.1455201549003.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...