After final painting you can only measure the final paint DFT.
If you needed DFT after primer and first coat then you should have checked earlier.
Regards
Prem Nautiyal
Sent from Samsung Mobile
-------- Original message --------
From: Dinesh Somwanshi
Date:03/02/2016 11:31 AM (GMT+05:30)
To: materials-welding
Subject: Re: [MW:24218] Re: Painting DFT guage for individual layer reading.
Dear ,
I want indivisual reading of primer , intercoat & final reading of DFT for applied paint systems.
Regards
dinesh
DINESH VITTHAL SOMWANSHI
BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135
असो द्यावी दया तुमच्या लागतसे पाया.
Pray for others, sometime, You might never need to pray for yourself again.....
On Wed, Feb 3, 2016 at 10:45 AM, Mohd Siraj <mohd52100@gmail.com> wrote:
question not clear.--you mean by type of DFT gauge to be used for layers?
On Wednesday, February 3, 2016 at 7:20:08 AM UTC+3, dinesh AWS-CWI ,CSWIP 3.1,NDT II wrote:Dear WI / PI,s,Please provide details of available Painting Guage to define individual paint layer DFT for multi layer paint system.DINESH VITTHAL SOMWANSHIBACHELOR IN MECHANICAL ENGINEERAUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,AWS - CWI , CSWIP 3.1BGAS Gr 2 / 3NDT II -UT , RT , MT , PT, VTअसो द्यावी दया तुमच्या लागतसे पाया.Pray for others, sometime, You might never need to pray for yourself again.....
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/43d65839-106c-429a-a94f-6b1331f6716b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVPRD1PiQfCKcT1d-DPiZecvK6W1W34Cgx%2B7fS-KdbPqg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment