[MW:24260] Re: How to protect Serration of Flanges during Hot dip galvanization

Does any one know how could i remove the hot galvanized coating from face of flange?
plz advise


On Monday, August 23, 2010 at 1:08:56 PM UTC+4:30, aly mhaskar wrote:


Dear All,
Presently we are doing hot dip galvanization of pipe spools where we have to protect the serration of flanges during galvanization.
 
Can any body suggest what can be applied on serration to protect it from adhesion of ZINC on serration.
 
Thank you in advance.
 
Mhaskar Aly
Kuwait




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/75d1da68-c97b-4709-b526-afb7cfd25136%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...