Dear Experts,
we have Incoloy 825 cladded pipes.
Due to some bad handling, some scratches are observed on the cladded CRA portion. The scratch is maximum 0.3 mm deep
We want to smoothen/ dressing it using the emery paper. Which type of emery is suitable on the Incoly 825 CRA. Will the Carbide in the emery paper will damage the CRA?

Can you please advise any other suitable method to remove the scratch marks.

--
Thanks and Best regard
Kumar


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK9xe5XrWd8p5gZOxyY9oJ-XkHRevLty2A2Uubq24%2BXwjtrmYg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...