We have to fire proof somE steel structure profiles
However, in the meantime our client's SPC calls for Hot Dip Galvanized
Is intumescent fire proofing paint compatible with HDG?
Anyone has range of price/SQM for intumescent paint?
Thanks
--
Sent from Gmail Mobile
--