Skip to main content

Re: [MW:23849] Re: ASTM A36 plates for pressure vessels

dear Syed, 

strictly,code, there is no limitation on raw material for the products to be certified as per A 234, except it shall meets with chemical requirements of particular grade. 
If specific requirements based on service (like NACE), then restricted chemistry applies. 

regards, 

jignesh rana 

On Tue, Nov 3, 2015 at 11:50 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
In addition Code Case 2811 provides guidelines for use of  SA/EN 10025-2 Steel Grades S235J2, S275J2, and S355J2   in fabrication of pressure vessels

https://www.linkedin.com/grp/post/122787-6061068041251278851?trk=groups-post-b-title

On 3 November 2015 at 10:12, Abhay Pethe <agpethe@gmail.com> wrote:
SA-36 is permitted for use in construction of pressure vessels according to UCS-6 of the ASME BPVC. Practically nobody uses the same remains the fact.

No comments regarding the equivalency or use of A36 in place of A234.


Best Regards,
Abhay Pethe

On 30 October 2015 at 06:54, Plate Steel <eric@ysteelplate.com> wrote:
Dear Syed,

Firstly A36 is just one common carbon structural steel,this steel plate can make common tanks,but not pressure vessels.Because,As a professional steel supplier,we knew when rolling A36,no need to do Ultrasonic test,but for pressure vessel used steel,they have to be done Ultrasonic test.

Second,your said A234 is one pressure vessel steel,actually another pressure vessel steel ASTM A285GrC is similar to A234.

It would be dangerous if using A36 to replace of A234,Freind.

Eric 

在 2011年1月24日星期一 UTC+8下午9:36:28,Moin - QC写道:

Dear members,

Can a plate to ASTM A36 can be used to manufacture TEEs to A234 WPB, is there any restriction in BPV or B31.3 on the use of A36 plate for manufacturing A234 Tees.

One of client says A36 is for general purpose and cannot be used for making a pressure containing component to be used in oil and gas production . Is it correct, if yes why? And if not can you please provide me a technical justification, I could not find anything B31.3.

Thanks & Regards
Syed Moin                               


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubm111HFHayhmwPOOyE7K34hOjbhuG8gizMFi1yj%2BX4CmQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKB7vAJwAZT173V-HTtswhPE6Ng%2BPunoWW4VXSA%2B7%3D%3D1Db-%3DGA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...