Re: [MW:23928] Tensile testing

Dear Mr. Alan

 Thermo-mechanical controlled processed micro allying steel resist the dislocation motion for certain period of time but shows the Luders band of yeild point in very short area. 
Recently, new methods have been started to be used for investigation of plastic flow of metals such as thermography please see the attachement of ;
1) Influence of Niobium on the Beginning of the Plastic Flow of Material during Cold Deformation.
 
2) For reference 3% Ni steel -Normalised+ Acc. Cooled+ Tempered.( Its shows the Yeild point)


Please clarify your suggestion

On Monday, November 16, 2015 at 1:32:48 PM UTC+3, alan wrote:
I have to comment, since  I do not agree that 'the yield point is observed in all carbon steel material'  [but it may depend on what you consider to be a carbon steel]. That statement is probably true for as-rolled and normalised carbon steels but, notably, the TMCP [thermo-mechanical controlled processed] steels which are carbon-manganese micro-alloyed steels and widely used for structures and pipelines do not generally show a distinctive yield point.

Alan Denney
AKD Materials Consulting Ltd
-----Original Message-----
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Pravin Nimbalkar
Sent: 16 November 2015 07:14
To: Materials & Welding <material...@googlegroups.com>
Subject: Re: [MW:23883] Tensile testing

Definitely

construct a straight line parallel to the initial linear portion of the stress-strain curve, but offset from it by e = 0.002 (0.2%.) The yield strength is taken as the stress level at which this straight line intersects the stress–strain curve.

Generally the yield point is observed in all carbon steel material.
The reason behind yield point is Cottrell atmosphere. Its related to how dislocation pinned in mild steel metals by carbon and nitrogen interstitials. These atoms distort the lattice shortly and there will be associated residual stress field surrounding the interstitials. This stress field relaxed by interestitail atoms diffusing towords dislocation. Once the dislocation has become pinned a small extra force is required to unpinn and the dislocation prior the yielding and produce upper yield point in stress-strain strain diagram. After unpinning dislocation are free to move in Crystal which results means lower yield point and material will deform in more plastic manner.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca4a0665-8653-4b56-8c30-72e4b23d9a9d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b0ca89bc-307e-4d9f-808b-d9795ba776ac%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...