RE: [MW:23852] Re: ASTM A36 plates for pressure vessels

To All,

 

A small correction in my response as below.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist

Hamilton, Ontario, Canada

pgoswami@quickclic.net

pradip.goswami@gmail.com

ca.linkedin.com/pub/pradip-goswami/5/985/299


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Tuesday, November 03, 2015 11:52 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:23850] Re: ASTM A36 plates for pressure vessels

 

Hello Syed,

 

You should  NOT use A-36 steel for making fittings. Please see the materials requirements for A 234 fitting vs. the Scope for A-36 material. The text narrated below  is self explanatory. Any killed grade of C-Mn steel would be a good substitute for A-36 subject to the design requirements.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist

Hamilton, Ontario, Canada

pgoswami@quickclic.net

pradip.goswami@gmail.com

ca.linkedin.com/pub/pradip-goswami/5/985/299

 

SA-234/SA-234M

 

Materials 5.1 The material for fittings shall consist of killed steel, forgings, bars, plates, seamless or fusion-welded tubular products with filler metal added and shall conform to the chemical requirements of Table 1. Unless otherwise specified for carbon steel plates, the steel may be made to either coarse grain or fine grain practice

 

SA-36/SA-36M:-

1. Scope

1.1 This specification covers carbon steel shapes, plates, and bars of structural quality for use in riveted, bolted, or welded construction of bridges and buildings, and for general structural purposes


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of JIGNESH RANA
Sent: Tuesday, November 03, 2015 11:33 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:23849] Re: ASTM A36 plates for pressure vessels

 

dear Syed, 

 

strictly,code, there is no limitation on raw material for the products to be certified as per A 234, except it shall meets with chemical requirements of particular grade. 

If specific requirements based on service (like NACE), then restricted chemistry applies. 

 

regards, 

 

jignesh rana 

 

On Tue, Nov 3, 2015 at 11:50 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:

In addition Code Case 2811 provides guidelines for use of  SA/EN 10025-2 Steel Grades S235J2, S275J2, and S355J2   in fabrication of pressure vessels

 

https://www.linkedin.com/grp/post/122787-6061068041251278851?trk=groups-post-b-title

 

On 3 November 2015 at 10:12, Abhay Pethe <agpethe@gmail.com> wrote:

SA-36 is permitted for use in construction of pressure vessels according to UCS-6 of the ASME BPVC. Practically nobody uses the same remains the fact.

 

No comments regarding the equivalency or use of A36 in place of A234.


 

Best Regards,

Abhay Pethe

 

On 30 October 2015 at 06:54, Plate Steel <eric@ysteelplate.com> wrote:

Dear Syed,

 

Firstly A36 is just one common carbon structural steel,this steel plate can make common tanks,but not pressure vessels.Because,As a professional steel supplier,we knew when rolling A36,no need to do Ultrasonic test,but for pressure vessel used steel,they have to be done Ultrasonic test.

 

Second,your said A234 is one pressure vessel steel,actually another pressure vessel steel ASTM A285GrC is similar to A234.

 

It would be dangerous if using A36 to replace of A234,Freind.

 

Eric 

在 2011年1月24日星期一 UTC+8下午9:36:28,Moin - QC写道:

Dear members,

Can a plate to ASTM A36 can be used to manufacture TEEs to A234 WPB, is there any restriction in BPV or B31.3 on the use of A36 plate for manufacturing A234 Tees.

One of client says A36 is for general purpose and cannot be used for making a pressure containing component to be used in oil and gas production . Is it correct, if yes why? And if not can you please provide me a technical justification, I could not find anything B31.3.

Thanks & Regards
Syed Moin                               

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubm111HFHayhmwPOOyE7K34hOjbhuG8gizMFi1yj%2BX4CmQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKB7vAJwAZT173V-HTtswhPE6Ng%2BPunoWW4VXSA%2B7%3D%3D1Db-%3DGA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...