RE: [MW:23711] Backing Gas for SS Pipe Welding

If material P No. is not falling as mentioned in QW-408.9 then backing gas is non essential variable as per ASME SEC.IX so it doesn't require requalification

On 12 Oct 2015 20:36, "John Henning" <jhenning@deltak.com> wrote:

Depends on the Code and the process.

 

For Section IX, GTAW:  addition or deletion of backing gas or a change in flow rate of the backing gas is a non-essential variable.  It must be addressed on the WPS but can be changed without any requalification.

 

 

If you are unfamiliar with ASME IX, first column are essential variables (changes require requalification), 2nd column are supplementary essential variables (apply if impact qualification is required), and third column are nonessential – variables that must be addressed on the WPS but can be changed.

 

So, technically, the WPS meets Sc IX if addressed as none.  But, stainless steel should be gas backed or back gouged and welded (except in very specific instances) to prevent oxidation of chromium at the root of the weld.

 

Hope this helps.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of navnitkumar parikh
Sent: Monday, October 12, 2015 8:23 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:23707] Backing Gas for SS Pipe Welding

 

Dear

Deletion of backing gas is an essential varible so if PQR qualified with backing gas then mention backing gas in WPS.

Regards,
Navnitkumar Parikh
Asst. Manager-Welding
Thermax Limited

On 12 Oct 2015 18:39, "pras ari" <alhanif.pras@gmail.com> wrote:

Dear Experts,

I have read WPS/PQR and I found that on PQR mentioned use backing gas (argon) with argon but on WPS without backing gas (argon).

Please advise to me, this WPS/PQR approved or not?

Thanks & Regards

Winarko

winarko@pp-epc.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwoFc8fsYB2f5QpOGcnQ4OJNMYagk3_1DVK%3DLMw5%3D_9f%2Bw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHZGHr61dTyejdBeRLVdaifGQOUqS%3DasAujc7EdoPz%3D%2BNH9og%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BY2PR0301MB1541A3E644294A0E3D66B34EA1310%40BY2PR0301MB1541.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHZGHo0UZBsdcT45LE%2BP3u1gm3uVNxN2dJ42y96KM5kqs0EQQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...