Hi,

Go for your client request because why their asking not performing HT of that line, that is the main reason.

Regards
Venkat

On Thu, Oct 8, 2015 at 5:50 PM, 'sugu puma' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear gentleman,

I have some doubt regarding 2inch pipe require 100% RT, in isometric drawing already state 10% only RT. Code b31.3
This line not test with hydrotest but its going to replace with pnumatic test, final stages client was request 100%RT,
Please friends,any possible to do this requirement,or any solution to out get reduce the requirement

Hope hearing from you soon,

Cheers.....

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1444315857.27701.YahooMailAndroidMobile%40web162606.mail.bf1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsM-MWpz1hu1XxK%3DuoOkAZxp2Y5tBwgVt_2AibX_znG2Sw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...