Wednesday, October 7, 2015

Re: [MW:23679] SS to BRASS Welding

Hi

Please use silver brazing alloy and proceed with brazing.

Regards

Prem Nautiyal



From: Naveen Raj <mecnaveen90@gmail.com>
Sent: Wed, 07 Oct 2015 11:51:33
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:23674] SS to BRASS Welding
Dear All,

Kindly advise me what welding material will be used to joint SS 304 to BRASS.

We used copper soldering method but the SS tube broken after welding..

Thickness of SS is 0.8mm. Pls find the picture...

Thanks in advance....

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7051d20a-a6e8-4e84-afee-5d6cb653692c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1444198893.S.184890.11731.f4-234-233.1444241814.14578%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...