Re: [MW:23656] L.O.P Criteria according to AWS D1.1

Dear Mehdi,

Referring to AWS D1.1 Table 6.1 "Complete  fusion shall exist between adjacent layers of weld metal and between weld metal and base metal" but if the joint welding symbol mentioned CJP, BG, FP then no acceptance criteria for LOP.



-- 
Best regards,
 
Tarek Yehia
Cell#:  00966 50 104 0991
           00966 56 772 6160
Skype ID: eng.cardo@skype.com


On Sat, Oct 3, 2015 at 1:23 PM, Mehdi Vafakhah <mehdi.vafakhah@gmail.com> wrote:
 Dear experts

whats the L.O.P Visual Inspection Acceptance Criteria according to AWS D1.1 ?

Best regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/60468822-24e4-4a64-8127-db4fde3a250a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOpHpqCXOcJbkanKpVsjZppbFt1P7i8mH0Hz1z3%3DeL%2Bb4LFwoA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...