Dear Experts,
Please advice what the minimum butt weld passes or weld % shall comleted before leave the weld to cool to imbient temperature and the practice to do if exist such as preheat and surface test, design code API1104.
I believe that as per DEP Shell Spec. It allow the weld after third pass to cool to imbient temp. without mention any such practice.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGQQyUZ0S4ysA-c4vk62FRTD21gDu8ZwbXr6Qqds1gP2vjsGmA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...