Generally RT ,All weld-test with impact and one chemical pad is sufficient
-- Thanks
Vinay Tripathi
9643886124
On Wednesday, September 30, 2015 at 9:40:00 AM UTC+5:30, mohan raj v wrote:
On Wednesday, September 30, 2015 at 9:40:00 AM UTC+5:30, mohan raj v wrote:
Dear All,
Please clarify for electrode qualification test as per ASME Sec II Part C for E7018 Dia-4 mm, what are the test requirements?.As per Table 4, Fillet weld test piece is required for chemical analysis, RT, All-weld test & Impact test. Please clarify what table 4 is stating.Further, if i make one Groove weld test assembly of 20 mm thick, is it sufficient for the electrode qualification?Thanks & Regards,Mohan Raj
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ff7a1ca5-7a26-4e4d-a620-c0f8be846ebb%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment