A PQR was qualified with a test coupon of 22mm and in reference WPS the thickness range is given as 13-44 mm. Upon raising query it was informed that this WPS would only be used for welding of plates in the thickness range of 13-44. Is it correct or theoretical thickness range as per Table 451.1 of ASME sec IX should have been mentioned. please reply