Tuesday, April 7, 2015

Re: [MW:23051] Magnetization of A 335 P11/P12 during grinding process

Do preheat before welding do demagnetize it

On Tue, Apr 7, 2015 at 2:54 PM, Don Under Survilliance <donsaab3@gmail.com> wrote:
wrap the copper coils around the job at location and ground it. it will surely help
 

On Tue, Apr 7, 2015 at 12:36 PM, B Osare <bosare@nfl.co.in> wrote:
Dear Experts,
 
We have observed that piping material  A 335  P11 & P12 of Super heater Header Tee size 12"& 18" (Thickness 45.00 mm & 65.00 mm respectively)  was magnetized during grinding process at Location (not in workshop).   Can anyone tell us how this phenomenon occurs and how it can be de-magnetize at job location? The weld material is getting cracked after welding. Please suggest the  welding procedure with suitable welding electrodes & what precautions  to be taken during welding.
 
 
Regards
 
B Osare
From National Fertilizers Limited, Vijaipur

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CE2FEBA545354C0C93B2B0585FD87FE4%40mechworkshop.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM6T1-EfX8LRSJaUtwXSOD4ad7Y0764eXLW00OwpRRofD8qQ7w%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRLdY9rMveU9_zzDKXmBT9PPKbMusoBs1S170R4Fo9SpXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...