GOOD MORNING........
During fit up inspection of Partial penetration single bevel (PJP) found root gap between 1.5 to 3 mm in modular structure. Whether is it acceptable root rap or not .Company asked to rectify above said the joints. Please advise me if someone knowns about this.
Note –I know that full penetration required root gap and does not required in Partial penetration single bevel apart from this any code say,please guide me regarding this issue.
Regards
Bijaya Gouda
Lead QC Inspector
(welding & structure)
Get your own FREE website, FREE domain & FREE mobile app with Company email. | Know More > |
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150409044405.11107.qmail%40f4mail-235-219.rediffmail.com.