Re: [MW:22793] Preheat temperature for super duplex WPS (pipe 6" THK 22mm S32760)

NO NEED PREHEAT
 

 
On Tue, Feb 3, 2015 at 7:09 AM, tinhaminhvt ha <tinhaminhvt@gmail.com> wrote:
Dear all,

I didn't find any information for Preheat temperature for super duplex WPS (pipe 6" THK 22mm S32760) on ASME B31.1 or ASME IX, can anybody help me?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b3e998f0-8ece-46ee-9fd9-facec1b94cc8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGYkEe1_MtODFO7FuCvgeRB6eStteYP2RwWjY_eVo2APu56JFg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...