Symbol indicates welding to be done 3 sides only as per the given template size..
Regards,
E Sateesh babu.
.
I have a question about a welding symbol that has been driving me crazy.
-- I am reviewing a shop drawing for a sub-contracted steel fabricator, and I can't for the life of me find any information on the tail symbol in their drawing, which I have highlighted in the attachment. It is welding an angle to a square HSS. The symbol is not covered in the CISC Handbook of Steel Construction, and I have looked all over the internet, to no avail.
Can anyone provide information on its meaning?? Additionally, I am very curious as to its origin, or where it is standardized.
- Curt
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/88e59918-824a-4115-a019-5a29c9547502%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ%2Btj08s%3DRNJGjU73L4_%3DDzArUyR6dbOo_sDby2%3DLX0TjfGp_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments