Thursday, January 22, 2015

Re: [MW:22747] Thickness Range for WPS

Pls refer QW403.6 for SMAW process, Impact testing. MY question is for CS material only not LTCS

Thickness range 1.5 mm to 2T or T/6 to 2T

Thanks & Regards,
Mohd. Azam

On Thu, Jan 22, 2015 at 3:18 PM, <george.dilintas@gr.bureauveritas.com> wrote:

Τ/2 to T + 6 (see table 323.3.1)
you will never find impact test qualification requirements and ranges  in Section IX. Always in the construction Code Section

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Mohd Azam ---22/01/2015 13:30:46---Dear Experts, The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & .

From: Mohd Azam <azam1976@gmail.com>
To: materials-welding@googlegroups.com
Date: 22/01/2015 13:30
Subject: [MW:22744] Thickness Range for WPS
Sent by: materials-welding@googlegroups.com





Dear Experts,
The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & . Thickness criteria is to followed as per ASME B31.3:
 
P. No. 1 GR.1 (A106 Gr.B) to  P. No. 1 Gr.2 (A105N),
Impact @ -20 Deg C as per project specification requirement
 
Thickness for WPS 1.5 mm to 20 (T to 2T) mm or 5 to 16 mm (T/2 to T+6).
 
Kindly give the code reference:
 
 
Thanks & Regards,
Mohd. Azam

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CABD%2BRXS46ip-dH%3Dg2d0P_AyhtA4PaWkVNavRCUT0YH%3DAWoGs0g%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFA9B1FC5D.6C8AB053-ONC2257DD5.004374EE-C2257DD5.004395F0%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXRx4%2B97SSGkMzVb%2BHRi3N5onEqkxA0DrDD7V2ZUbHxq9w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...