Re: [MW:22735] Welding of Cast iron+ SS316 L

Nickel based

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Praveen Kumar ---19/01/2015 12:03:22---Dear Sir, Could you please suggest me which suitable welding electrode we can use for

From: Praveen Kumar <praveenkumar.sek@gmail.com>
To: materials-welding@googlegroups.com
Date: 19/01/2015 12:03
Subject: [MW:22733] Welding of Cast iron+ SS316 L
Sent by: materials-welding@googlegroups.com





Dear Sir,
 
Could you please suggest me which suitable welding electrode we can use for dissimilar composition material of Cast iron & SS 316 L.
 
Looking forward your early reply.

Thanks & regards,

S.Praveen kumar
TATA projects Ltd 
Nellore 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CABJqOFNgaPkFVoG8tWhM79egREMVxQxqskC2oP2h8paJq0rRLA%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...