Impact test is not a requirement related to material or thickness or welding process or something like those.
It's your design code/Spec., which have to mention this requirement.

On Wed, Jan 14, 2015 at 2:27 PM, Sateesh Babu E <e.sateeshbabu@gmail.com> wrote:
Dear All,


Please provide ASME sec IX interpretation/clause to solve the below issue.

Backgorund:

Base metal-1 thk : 40 mm (IS 2062 Gr.B)
Base metal -2 Thk : 3 mm (IS 2062 Gr.A)

Filler wire : ER70S-6 (1.2 mm)
Gas : Co2.

Question : Base metal and deposited weld metal thickness range for the above combinations (Impact test is required) ?.






--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ%2Btj09ks%3DHmmOVu%2BujhoTJ7vPJm2yMSraevZdmcwCupTRP27A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtvYOv4UvKs0VVHhvR8%2Bdq9aYwEF9Uye3he3TGoNeoNCuw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...