Wednesday, January 14, 2015

Re: [MW:22722] Thin material welding

We may have to check the actual extent/ condition of damage in welds to evaluate the repairing possibilities.

S.N.Bagchi.


On Wednesday, January 14, 2015 12:43 PM, 'Neilashkumar' via Materials & Welding <materials-welding@googlegroups.com> wrote:


  Dear all,

We have a project for Seam Welding repairing work of Stainless steel
round duct piping for rubber finish building,details are as follows,
Total repairing welding length-500-550meter
Pipe material.    --EFW304/304LSS A240
Pipe thickness --below 3mm
Pipe size --0.75" -20"dia
Can you please tell me whether it is possible to do repair welding ? Method
to do repair weld.

P.NEILASHKUMAR
Sent from my iPad
MOB : 966 533098265
           91+9952110791


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/C90FF222-A0AB-466C-8E5C-313F24AFEBF2%40yahoo.com.

For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...