Re: [MW:22691] Hardness Value of Inconel 625

Hi,

It is not specified in code, if you refer to shell MESC, it is 32 HRC.

Sent from my iPhone

On Dec 31, 2014, at 10:06, LALU RAJENDRAN <lalucpt@gmail.com> wrote:

Dear Experts,

What is the hardness value of Inconel-625 (ASTM B444 UNS N06625)?


Regards,
LALU
LINKS MIDDLE EAST

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13t1W3GvM2xV6z3_D91J-DiUjTgwynS%3DL3qeCBOTPy2-Ng%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...