[MW:22744] Thickness Range for WPS

Dear Experts,

The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & . Thickness criteria is to followed as per ASME B31.3:

 

P. No. 1 GR.1 (A106 Gr.B) to  P. No. 1 Gr.2 (A105N),

Impact @ -20 Deg C as per project specification requirement

 

Thickness for WPS 1.5 mm to 20 (T to 2T) mm or 5 to 16 mm (T/2 to T+6).

 

Kindly give the code reference:

 

 

Thanks & Regards,

Mohd. Azam

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXS46ip-dH%3Dg2d0P_AyhtA4PaWkVNavRCUT0YH%3DAWoGs0g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...